Effect of Annealing at High Temperatures on Microstructural Formation of 15Cr-25Ni Austenitic Stainless Steel Cast

- Syahbuddin (1), - Parikin (2), Mohammad Dani (3), Salim Mustofa (4), Andon Insani (5), Eddy Agus Basuki (6), Ching An Huang (7)
(1) Department of Mechanical Engineering, Faculty of Engineering, Universitas Pancasila, Srengseng Sawah, Jakarta 12640 Indonesia
(2) Center for Science and Technology of Advanced Materials, National Nuclear Energy Agency, Puspiptek Area, Banten 15314, Indonesia
(3) Center for Science and Technology of Advanced Materials, National Nuclear Energy Agency, Puspiptek Area, Banten 15314, Indonesia
(4) Center for Science and Technology of Advanced Materials, National Nuclear Energy Agency, Puspiptek Area, Banten 15314, Indonesia
(5) Center for Science and Technology of Advanced Materials, National Nuclear Energy Agency, Puspiptek Area, Banten 15314, Indonesia
(6) Department of Metallurgical Engineering, Bandung Institute of Technology, Jl. Ganesha No.10, Bandung, Indonesia
(7) Department of Mechanical Engineering, Chang Gung University, Taoyuan, Taiwan
Fulltext View | Download
How to cite (IJASEIT) :
Syahbuddin, -, et al. “Effect of Annealing at High Temperatures on Microstructural Formation of 15Cr-25Ni Austenitic Stainless Steel Cast”. International Journal on Advanced Science, Engineering and Information Technology, vol. 11, no. 3, June 2021, pp. 1042-8, doi:10.18517/ijaseit.11.3.10456.
Microstructure of 15Cr-25Ni Austenite stainless steel (ASS) cast formed at various high temperatures has been investigated in this study. The steel was synthesized from scrap materials containing Cr and Ni elements, respectively, about 15 and 25 wt.%. This steel designed to have high corrosion resistance or high-temperature oxidation is a steel candidate for evaporator materials in a waste incinerator, and their operating temperature is used for annealing temperatures in this study. The variation of annealing temperatures was carried out at temperatures of 400, 600, 800, 950, and 1078°C for a time of 30 minutes. The ASS as-cast and annealed have a similar microstructure dominated by the dendritic structure of γ-FeNi austenite with the crystal structure of the face-centered cubic interdendritic region of a eutectic structure containing free particle zone and (Fe, Cr)7C3 island compounds. The short dendritic arm spacings for ASS after annealing at temperatures of 400, 600, and 800°C were measured to have about 61.71, 62.11, and 57.85 mm, respectively.  By contrast, the longer dendritic arm spacings were obtained after annealing at temperatures of 950 and 1078°C about 70.29 and 197.04 μm, respectively.  In addition to higher micro-strains, the short dendritic arm spacings formed after annealing at 400-800° C lead in a relatively higher hardness profile, whereas the longer dendritic arm spacings obtained after annealing at 950 and 1078°C result in a low hardness profile in the ASS.

Abdalla,A.M., Hossain,S., Petra,P.M., Ghasemi,M. Azad,A.K., Achievements and trends of solid oxide fuel cells in clean energy plane: a perspective review. Front. Energy 1-24, 2018. https://doi.org/10.1007/s11708-018-0546-2.

Manal, A. S. Optimization of Multiple Effect Evaporators Designed for Fruit Juice Concentrate. Am. J. of Energy Eng. Special Issue: Energy Conservation in Food Industry. Vol. 3, No. 2-1, pp. 6-11, 2015. doi: 10.11648/j.ajee.s.2015030201.12

Setyawan, A. and Sujati, N. M., Evaluasi hasil analisis efisiensi kinerja sistem evaporator IPLR tahun 2014-2017, Prosiding Seminar Nasional Teknologi Pengelolaan Limbah XV, p. 255-259, 2017.

Effendi,N. Darwinto, T., Parikin et al., Indonesian J. of Mat. Sci. 15 4, 187, 2014.

Parikin, Dani, M., Sukaryo, S. G. 2019. Review on A New Austenitic 57Fe15Cr25Ni Stainless Steel at Temperature of 850ï‚°C for 30 Minutes Followed by Water Quenching Treatments. Malaysian Journal of Fundamental and Applied Sciences Vol.p, No.q, pp. x-y. accepted

Parikin, M.Dani, A.K. Rivai, A.Dimyati, Syahbuddin, C.A. Huang, Effect of Different Cooling Rates on Mechanical Strength OF 56Fe16Cr25Ni Austenitic Stainless Steel After Heat Treatments at 850ï‚°C for 30 Minutes, Makara Journal of Technology, Vol. p-q, x-y, accepted, 2020

P.J.G. Nieto, V.M.G. Suí¡rez, J.C.A. Antón et al., Materials 8, 3562, 2015.

Parikin, Dani M., Jahja A.K., Iskandar R., Mayer J., Crystal Structure Investigation of Ferritic 73Fe24Cr2Si0.8Mn0.1Ni Steel for Multipurpouse Structural Material Applications, International Journal of Technology 1: 78-88, 2018.

Parikin, Ismoyo, A.H., Iskandar, R., Dimyati, AMicrostructures and Hardness of TIG Welded Experimental 57Fe15Cr25Ni Steel, Makara Journal of Technology, University of Indonesia vol. 22/2, pp. 66-71, 2018.

Parikin, Dani M., Ismoyo A.H., Dimyati A., Microstructures and Hardness of the Experimental 57Fe15Cr25Ni Austenitic Steel around the TIG Weld-Joints, Makara Journal of Technology-University of Indonesia, 22/2 66-67, 2018.

L. Lutterotti, MAUD tutorial-instrumental Broadening Determination, Dipartimento di Ingegneria dei Materiali, Universita di Trento 38050 Trento, Italy, pp. 1-18, 2006.

M. Kadziolka-Gawel, W. Zarek, E. Popiel and Chrobar, The Crystal Structure and Magnetic Properties of Selected fcc FeNi and Fe40Ni40B20 Alloys, Acta Physica Polonica A, 117 (2) 412-414, 2010.

M.Dani, S. Mustopa, Parikin, Sumaryo, T. Sudiro, B. Hermant, D. R. Adhika, A. Dimyati, Syahbuddin, Sri Hardjanto, E. A. Basuki, C. A. Huang, Effect of Spark Plasma Sintering (SPS) at temperature of 900C and 950ï‚°C for 5 Minutes on Microstructural Formation of Fe-25Ni-17Cr Austenitic Stainless Steel, International Journal of Emerging Trends in Engineering Research, 8(8), 4845 - 4853, 2020.

S. Mustopa, M.Dani, Parikin T. Sudiro, B. Hermanto, D. R. Adhika, Syahbuddin, C. A. Huang, Effect of Temperature of Spark Plasma Sintering on the Development of Oxide Compoundin the Fe-25Ni-17Cr Austenitic Stainless Steel, International Journal of Emerging Trends in Engineering Research, 8(9), 5661-5667, 2020.

M. Dani, A. Dimiyanti, Parikin, D.R. Adhika, A.K. Jahja, A. Insani, Syahbuddin, C.A. Huang, Microstruture and Deformation of 57Fe17Cr25NiSi Austenitic Super Alloy After Arc Plasma Sintering, International Journal of Technology 10(5), 988-998, 2019.

K. Wieczerzak, P. Bala, M. Stepien, G. Cios, T. Koziel, The Characterization of Cast Fe-Cr-C Alloy, Archives of Metallurgy and Materials, Volume 60 (2) 779-782, 2015.

Majid Abbasi, Mahdich Yahdatnia and Ali Navael, Solidification Microstructure of HK Resistant Steel, International Journal of Metal Casting, 9(4), 19-26, 2015.

Francisco J.G. Silva, Jorge Santos, and R. Gouveia, Dissolution of Grains Boundary Carbide by the Effect of Solution Annealing Heat Treatment and Aging Treatment on Heat-Resistant Cast Steel HK30, Metals 251(7), , 1-12, 2017

EA Kenik, J.T. Busby, D.T. Hoelzer, A.F. Rowecliffe, and J.M. Vitek, Microstructure and Elemental Distribution in a Cast Austenitic Steel, Microsc. Microanal. 13(2), 2007.

Creative Commons License

This work is licensed under a Creative Commons Attribution 4.0 International License.

Authors who publish with this journal agree to the following terms:

    1. Authors retain copyright and grant the journal right of first publication with the work simultaneously licensed under a Creative Commons Attribution License that allows others to share the work with an acknowledgement of the work's authorship and initial publication in this journal.
    2. Authors are able to enter into separate, additional contractual arrangements for the non-exclusive distribution of the journal's published version of the work (e.g., post it to an institutional repository or publish it in a book), with an acknowledgement of its initial publication in this journal.
    3. Authors are permitted and encouraged to post their work online (e.g., in institutional repositories or on their website) prior to and during the submission process, as it can lead to productive exchanges, as well as earlier and greater citation of published work (See The Effect of Open Access).